Mara® Poly P.
Bright colors for long-term outdoor use
Mara Poly P is a highly versatile screen printing ink. It enables high-quality printing for long-term outdoor use and on items such as beverage crates or transport containers made of PE and PP. Two-component system, can also be used as a protective coating on one-component ink systems.
- Glossy with high opacity
- Fast drying enables high printing speeds
- Chemical and weather resistant
- Surface insensitive



Substrates:
- Polyproylen (PP), treated
- Polyethylene (PE), pre-treated
- PVC, rigid
- Polyamide (PA)
- Anodised aluminium
Industry solution for:
- Bottle crates of PE and PP
- Transport Containers of PE and PP
- and much more
Highlights:
- Glossy with high opacity
- Fast drying enables high printing speeds
- Chemical and weather resistant
- Surface insensitive
Overprint Varnish

32100057910
Lemon
Light Yellow
Medium Yellow
Orange
Vermilion
Scarlet Red
Carmine Red
Magenta
Brown
Violet
Ultramarine Blue
Medium Blue
Brilliant Blue
Blue Green
Grass Green
White
Black
Overprint Varnish, with UV-Absorber
Milky Matt Varnish

32100057920

32100057922

32100057924

32100057926

32100057930

32100057932

32100057934

32100057936

32100057940

32100057950

32100057952

32100057954

32100057956

32100057960

32100057962

32100057970

32100057980

32100057911

32100057913
- Further Products910
Overprint Varnish
Overprint Varnish 910, 500 G
32100057910 - Basic Shades920
Lemon
922Light Yellow
924Medium Yellow
926Orange
930Vermilion
932Scarlet Red
934Carmine Red
936Magenta
940Brown
950Violet
952Ultramarine Blue
954Medium Blue
956Brilliant Blue
960Blue Green
962Grass Green
970White
980Black
Further Products911Overprint Varnish, with UV-Absorber
913Milky Matt Varnish
Lemon 920, 800 G
32100057920
Light Yellow 922, 800 G
32100057922
Medium Yellow 924, 800 G
32100057924
Orange 926, 800 G
32100057926
Vermilion 930, 800 G
32100057930
Scarlet Red 932, 800 G
32100057932
Carmine Red 934, 800 G
32100057934
Magenta 936, 800 G
32100057936
Brown 940, 800 G
32100057940
Violet 950, 800 G
32100057950
Ultramarine Blue 952, 800 G
32100057952
Medium Blue 954, 800 G
32100057954
Brilliant Blue 956, 800 G
32100057956
Blue Green 960, 800 G
32100057960
Grass Green 962, 800 G
32100057962
White 970, 800 G
32100057970
Black 980, 800 G
32100057980
Overprint Varnish, with UV-Absorber 911, 800 G
32100057911
Milky Matt Varnish 913, 800 G
32100057913
Properties:
- Screen Printing Ink for pre-treated polyethylene (PE) and polypropylene (PP), coated and powder-coated substrates
- Glossy, high opacity, fast drying 2-component ink system, resistant to chemicals, weather resistant, insensitive surface
Substrates:
- Polyproylen (PP), treated
- Polyethylene (PE), pre-treated
- PVC, rigid
- Polyamide (PA)
- Anodised aluminium
Auxiliaries:
| H1 | Hardener | 12.5 - 20 % |
| PV | Thinner | 10 - 20 % |
| MP | Matting Powder | 0.5 - 4 % |
| VM2 | Levelling Agent | 0.5 - 1 % |
| UR3 | Cleaner (flp. 42°C) | |
| UR4 | Cleaner (flp. 52°C) | |
| UR5 | Cleaner (flp. 72°C) | |
| P2 | Primer | |
| SV5 | Retarder | |
| SV10 | Retarder |
Ink adjustment:
All basic shades except Overprint Varnish:
800 g Mara®Poly P +
100 g (= 12,5 %) H 1
Overprint Varnishes P 910/911/913:
500 g Mara®Poly P +
100 g (=20 %) H 1
If basic shades are mixed with Overprint Varnish P 910 the proper addition of hardener must be calculated in the correct ratio.
When using hardener, the processing and curing temperature must not be lower than 15 °C as irreversible damage can occur. Please also avoid high humidity for several hours after printing as the hardener is sensitive to humidity.
Pre-reaction time
It is recommended to allow the ink/ hardener mixture to pre-react for 15 min.
Pot life
The mixture ink/hardener is chemically reactive and must be processed within 8-12 h (if stored at 20 °C). Higher processing temperatures reduce the pot life. If the mentioned times are exceeded, the ink's adhesion and resistance may be reduced, even if the ink still seems processable.
By continuously adding freshly mixed ink plus hardener, the pot life can be extended up to 24 hours if working in 3 shifts with rather low ink throughput.
Drying:
The following standard values can be assumed concerning the progressive cross-linking reaction (Mesh 90-55, single print):
| Dryness degree | Temperature | Time |
| overprintable | 20 °C air drying | 20 min |
| overprintable | hot air drying | 4 min |
| scratch resist. | 20 °C | 3 h |
| cured | 20 °C air drying | 8 days |
| cured | 80 °C oven drying | 60 min |
The mentioned drying times are only guidelines as they depend on the printed ink film thickness, air humidity, drying conditions, and the selection of auxiliaries such as thinner and/or retarder.
If multicolour prints are dried with enforced heat between printing sequences (by hot air or infrared), the time for overprinting is reduced to approx. 3-4 min.
Due to extreme stress on crates and ink, we do not recommend flaming.
When drying with enforced heat of more than 150 °C, the heat influence must not exceed 5 min in order to avoid yellowing, especially with White 970. Generally an extended drying time is necessary when overprinting the ink.
The ink film underneath must not be completely cured when overprinted. If the ink film is dried at room temperature 20 °C, overprinting must be carried out within 8 h. We recommend overprinting as soon as possible, in order to guarantee a good adhesion between the ink layers.
Printing parameters:
- Polyproylen (PP), treated
- Polyethylene (PE), pre-treated
- PVC, rigid
- Polyamide (PA)
- Anodised aluminium
- Bottle crates of PE and PP
- Transport Containers of PE and PP
- and much more
- Glossy with high opacity
- Fast drying enables high printing speeds
- Chemical and weather resistant
- Surface insensitive
Substrates:
Industry solution for:
Highlights:
- Further Products910
Overprint Varnish
Overprint Varnish 910, 500 G
32100057910 - Basic Shades920
Lemon
922Light Yellow
924Medium Yellow
926Orange
930Vermilion
932Scarlet Red
934Carmine Red
936Magenta
940Brown
950Violet
952Ultramarine Blue
954Medium Blue
956Brilliant Blue
960Blue Green
962Grass Green
970White
980Black
Further Products911Overprint Varnish, with UV-Absorber
913Milky Matt Varnish
Lemon 920, 800 G
32100057920
Light Yellow 922, 800 G
32100057922
Medium Yellow 924, 800 G
32100057924
Orange 926, 800 G
32100057926
Vermilion 930, 800 G
32100057930
Scarlet Red 932, 800 G
32100057932
Carmine Red 934, 800 G
32100057934
Magenta 936, 800 G
32100057936
Brown 940, 800 G
32100057940
Violet 950, 800 G
32100057950
Ultramarine Blue 952, 800 G
32100057952
Medium Blue 954, 800 G
32100057954
Brilliant Blue 956, 800 G
32100057956
Blue Green 960, 800 G
32100057960
Grass Green 962, 800 G
32100057962
White 970, 800 G
32100057970
Black 980, 800 G
32100057980
Overprint Varnish, with UV-Absorber 911, 800 G
32100057911
Milky Matt Varnish 913, 800 G
32100057913
Available in these sizes / volumesFurther Products910Overprint Varnish
Overprint Varnish 910, 500 G
32100057910Basic Shades920Lemon
922Light Yellow
924Medium Yellow
926Orange
930Vermilion
932Scarlet Red
934Carmine Red
936Magenta
940Brown
950Violet
952Ultramarine Blue
954Medium Blue
956Brilliant Blue
960Blue Green
962Grass Green
970White
980Black
Further Products911Overprint Varnish, with UV-Absorber
913Milky Matt Varnish
Lemon 920, 800 G
32100057920
Light Yellow 922, 800 G
32100057922
Medium Yellow 924, 800 G
32100057924
Orange 926, 800 G
32100057926
Vermilion 930, 800 G
32100057930
Scarlet Red 932, 800 G
32100057932
Carmine Red 934, 800 G
32100057934
Magenta 936, 800 G
32100057936
Brown 940, 800 G
32100057940
Violet 950, 800 G
32100057950
Ultramarine Blue 952, 800 G
32100057952
Medium Blue 954, 800 G
32100057954
Brilliant Blue 956, 800 G
32100057956
Blue Green 960, 800 G
32100057960
Grass Green 962, 800 G
32100057962
White 970, 800 G
32100057970
Black 980, 800 G
32100057980
Overprint Varnish, with UV-Absorber 911, 800 G
32100057911
Milky Matt Varnish 913, 800 G
32100057913- Screen Printing Ink for pre-treated polyethylene (PE) and polypropylene (PP), coated and powder-coated substrates
- Glossy, high opacity, fast drying 2-component ink system, resistant to chemicals, weather resistant, insensitive surface
- Polyproylen (PP), treated
- Polyethylene (PE), pre-treated
- PVC, rigid
- Polyamide (PA)
- Anodised aluminium
Properties:
Substrates:
Auxiliaries:
H1 Hardener 12.5 - 20 % PV Thinner 10 - 20 % MP Matting Powder 0.5 - 4 % VM2 Levelling Agent 0.5 - 1 % UR3 Cleaner (flp. 42°C) UR4 Cleaner (flp. 52°C) UR5 Cleaner (flp. 72°C) P2 Primer SV5 Retarder SV10 Retarder Ink adjustment:
The ink should be stirred homogeneously before printing and if necessary during production. Prior to printing, it is necessary to add hardener to the undiluted ink in the proper mixing ratio:
All basic shades except Overprint Varnish:
800 g Mara®Poly P +
100 g (= 12,5 %) H 1
Overprint Varnishes P 910/911/913:
500 g Mara®Poly P +
100 g (=20 %) H 1
If basic shades are mixed with Overprint Varnish P 910 the proper addition of hardener must be calculated in the correct ratio.
When using hardener, the processing and curing temperature must not be lower than 15 °C as irreversible damage can occur. Please also avoid high humidity for several hours after printing as the hardener is sensitive to humidity.
Pre-reaction time
It is recommended to allow the ink/ hardener mixture to pre-react for 15 min.
Pot life
The mixture ink/hardener is chemically reactive and must be processed within 8-12 h (if stored at 20 °C). Higher processing temperatures reduce the pot life. If the mentioned times are exceeded, the ink's adhesion and resistance may be reduced, even if the ink still seems processable.
By continuously adding freshly mixed ink plus hardener, the pot life can be extended up to 24 hours if working in 3 shifts with rather low ink throughput.Drying:
Parallel to physical drying, i. e. evaporation of solvents used, the actual hardening of the ink film is caused by the chemical cross-linking reaction between ink and hardener.
The following standard values can be assumed concerning the progressive cross-linking reaction (Mesh 90-55, single print):Dryness
degreeTemperature Time overprintable
20 °C
air drying20 min overprintable hot air drying 4 min scratch resist. 20 °C 3 h cured 20 °C
air drying8 days cured 80 °C
oven drying60 min
The mentioned drying times are only guidelines as they depend on the printed ink film thickness, air humidity, drying conditions, and the selection of auxiliaries such as thinner and/or retarder.
If multicolour prints are dried with enforced heat between printing sequences (by hot air or infrared), the time for overprinting is reduced to approx. 3-4 min.
Due to extreme stress on crates and ink, we do not recommend flaming.
When drying with enforced heat of more than 150 °C, the heat influence must not exceed 5 min in order to avoid yellowing, especially with White 970. Generally an extended drying time is necessary when overprinting the ink.
The ink film underneath must not be completely cured when overprinted. If the ink film is dried at room temperature 20 °C, overprinting must be carried out within 8 h. We recommend overprinting as soon as possible, in order to guarantee a good adhesion between the ink layers.Printing parameters:
All types of commercially available polyester and nylon fabrics and solvent-resistant stencils can be used. For a good opacity on dyed substrates, we recommend a fabric thickness between 68-64 and 90-48, for printing finest details 100-40 to 120-34.
CONTACT US
Marabu printing inks are used all over the world - with 16 subsidiaries worldwide and distribution partners in more than 80 countries. Find your contact here.