Mara® Flor TK.
Robust inks for outdoor textiles
The highly fade resistant pigmentation makes Mara Flor TK ideal for screen printing on outdoor textiles such as blinds, sunshades, workwear, and sailing fabrics. Solvent-based and two-component.
- High opaque ink system for synthetic and natural textiles
- High-quality pigmentation for long-term outdoor use applications such as blinds
- Wash-resistant up to 60°



Substrates:
- Polyamide (PA)
- Textile synthetics
- Cotton
Industry solution for:
- All types of synthetic textiles
- Workwear
- Sportswear
- Casual wear
- Umbrellas
Highlights:
- High opaque ink system for synthetic and natural textiles
- High-quality pigmentation for long-term outdoor use applications such as blinds
- Wash-resistant up to 60°
Opaque White
Lemon
Light Yellow
Medium Yellow
Orange
Vermilion
Scarlet Red
Carmine Red
Magenta
Brown
Violet
Ultramarine Blue
Medium Blue
Brilliant Blue
Blue Green
Grass Green
White
Black
Bronze Binder

33390057170

33390057920

33390057922

33390057924

33390057926

33390057930

33390057932

33390057934

33390057936

33390057940

33390057950

33390057952

33390057954

33390057956

33390057960

33390057962

33390057970

33390057980

33390057902
- High Opaque Shades170
Opaque White
Basic Shades920Lemon
922Light Yellow
924Medium Yellow
926Orange
930Vermilion
932Scarlet Red
934Carmine Red
936Magenta
940Brown
950Violet
952Ultramarine Blue
954Medium Blue
956Brilliant Blue
960Blue Green
962Grass Green
970White
980Black
Further Products902Bronze Binder
Opaque White 170, 1 kg
33390057170
Lemon 920, 1 kg
33390057920
Light Yellow 922, 1 kg
33390057922
Medium Yellow 924, 1 kg
33390057924
Orange 926, 1 kg
33390057926
Vermilion 930, 1 kg
33390057930
Scarlet Red 932, 1 kg
33390057932
Carmine Red 934, 1 kg
33390057934
Magenta 936, 1 kg
33390057936
Brown 940, 1 kg
33390057940
Violet 950, 1 kg
33390057950
Ultramarine Blue 952, 1 kg
33390057952
Medium Blue 954, 1 kg
33390057954
Brilliant Blue 956, 1 kg
33390057956
Blue Green 960, 1 kg
33390057960
Grass Green 962, 1 kg
33390057962
White 970, 1 kg
33390057970
Black 980, 1 kg
33390057980
Bronze Binder 902, 1 kg
33390057902
Properties:
- Screen printing ink for textiles made of synthetic and natural fabrics, polyurethane foam material
- Matt, semi-opaque, quick drying, 2 component ink system, weather and wash resistant
Substrates:
- Polyamide (PA)
- Textile synthetics
- Cotton
Auxiliaries:
| H2 | Hardener | 10 % |
| UKV1 | Thinner | 5 - 15 % |
| UKV2 | Thinner | 5 - 15 % |
| SA1 | Surface Additive | 3 - 5 % |
| STM | Thickening Agent | 1 - 2 % |
| SV1 | Retarder | |
| UR3 | Cleaner (flp. 42°C) | |
| UR4 | Cleaner (flp. 52°C) | |
| UR5 | Cleaner (flp. 72°C) |
Ink adjustment:
Mara Flor TK is a 2-component ink system. Prior to printing, it is essential to add hardener / adhesion modifier in the correct quantity and to stir homogeneously. When using hardener, the processing and curing temperature must not be lower than 15°C as irreversible damage can occur. Please also avoid high humidity for several hours after printing as the hardener is sensitive to humidity.
Pre-reaction time
It is recommended to allow the ink/hardener mixture to pre-react for 15 minutes.
Pot Life
The ink/hardener mixture is chemically reactive and must be processed within 8 h (referred to 20-25 °C and 45-60 % RH). Higher temperatures reduce the pot life. If the mentioned times are exceeded, the ink's adhesion and resistance may be reduced even if the ink still seems processable.
Drying:
| overprintable | 20 °C | 20 min |
| 60 °C | 5 min | |
| 120 °C | 3 min | |
| stackable | 20 °C | 60 min |
| 60 °C | 20 min | |
| 120 °C | 10 min | |
| final hardness | 20 °C | 5 days |
The times mentioned vary according to the substrate, the ink film thickness, the drying conditions and the selection of the auxiliaries used. Generally, an extended drying time is necessary when overprinting the ink. For multiple printing, please note that the film should not be completely cured before being overprinted.
If cured at a room temperature of 20 °C, the ink film has to be overprinted within 24 hours. Heat-activated intermediate curing is possible at 60 - 80 °C for 5 min.
Printing parameters:
All types of commercially available fabrics and solvent-resistant stencils can be used. We re-commend a fabric between 48–70 and 68-64.
- Polyamide (PA)
- Textile synthetics
- Cotton
- All types of synthetic textiles
- Workwear
- Sportswear
- Casual wear
- Umbrellas
- High opaque ink system for synthetic and natural textiles
- High-quality pigmentation for long-term outdoor use applications such as blinds
- Wash-resistant up to 60°
Substrates:
Industry solution for:
Highlights:
- High Opaque Shades170
Opaque White
Basic Shades920Lemon
922Light Yellow
924Medium Yellow
926Orange
930Vermilion
932Scarlet Red
934Carmine Red
936Magenta
940Brown
950Violet
952Ultramarine Blue
954Medium Blue
956Brilliant Blue
960Blue Green
962Grass Green
970White
980Black
Further Products902Bronze Binder
Opaque White 170, 1 kg
33390057170
Lemon 920, 1 kg
33390057920
Light Yellow 922, 1 kg
33390057922
Medium Yellow 924, 1 kg
33390057924
Orange 926, 1 kg
33390057926
Vermilion 930, 1 kg
33390057930
Scarlet Red 932, 1 kg
33390057932
Carmine Red 934, 1 kg
33390057934
Magenta 936, 1 kg
33390057936
Brown 940, 1 kg
33390057940
Violet 950, 1 kg
33390057950
Ultramarine Blue 952, 1 kg
33390057952
Medium Blue 954, 1 kg
33390057954
Brilliant Blue 956, 1 kg
33390057956
Blue Green 960, 1 kg
33390057960
Grass Green 962, 1 kg
33390057962
White 970, 1 kg
33390057970
Black 980, 1 kg
33390057980
Bronze Binder 902, 1 kg
33390057902
Available in these sizes / volumesHigh Opaque Shades170Opaque White
Basic Shades920Lemon
922Light Yellow
924Medium Yellow
926Orange
930Vermilion
932Scarlet Red
934Carmine Red
936Magenta
940Brown
950Violet
952Ultramarine Blue
954Medium Blue
956Brilliant Blue
960Blue Green
962Grass Green
970White
980Black
Further Products902Bronze Binder
Opaque White 170, 1 kg
33390057170
Lemon 920, 1 kg
33390057920
Light Yellow 922, 1 kg
33390057922
Medium Yellow 924, 1 kg
33390057924
Orange 926, 1 kg
33390057926
Vermilion 930, 1 kg
33390057930
Scarlet Red 932, 1 kg
33390057932
Carmine Red 934, 1 kg
33390057934
Magenta 936, 1 kg
33390057936
Brown 940, 1 kg
33390057940
Violet 950, 1 kg
33390057950
Ultramarine Blue 952, 1 kg
33390057952
Medium Blue 954, 1 kg
33390057954
Brilliant Blue 956, 1 kg
33390057956
Blue Green 960, 1 kg
33390057960
Grass Green 962, 1 kg
33390057962
White 970, 1 kg
33390057970
Black 980, 1 kg
33390057980
Bronze Binder 902, 1 kg
33390057902- Screen printing ink for textiles made of synthetic and natural fabrics, polyurethane foam material
- Matt, semi-opaque, quick drying, 2 component ink system, weather and wash resistant
- Polyamide (PA)
- Textile synthetics
- Cotton
Properties:
Substrates:
Auxiliaries:
H2 Hardener 10 % UKV1 Thinner 5 - 15 % UKV2 Thinner 5 - 15 % SA1 Surface Additive 3 - 5 % STM Thickening Agent 1 - 2 % SV1 Retarder UR3 Cleaner (flp. 42°C) UR4 Cleaner (flp. 52°C) UR5 Cleaner (flp. 72°C) Ink adjustment:
The ink should be stirred homogeneously before printing and if necessary during production.
Mara Flor TK is a 2-component ink system. Prior to printing, it is essential to add hardener / adhesion modifier in the correct quantity and to stir homogeneously. When using hardener, the processing and curing temperature must not be lower than 15°C as irreversible damage can occur. Please also avoid high humidity for several hours after printing as the hardener is sensitive to humidity.
Pre-reaction time
It is recommended to allow the ink/hardener mixture to pre-react for 15 minutes.Pot Life
The ink/hardener mixture is chemically reactive and must be processed within 8 h (referred to 20-25 °C and 45-60 % RH). Higher temperatures reduce the pot life. If the mentioned times are exceeded, the ink's adhesion and resistance may be reduced even if the ink still seems processable.Drying:
Parallel to physical drying, i. e. the evaporation of the solvents used, the actual hardening of the ink film is caused by the chemical cross-linking reaction between ink and hardener. The standard values concerning progressive cross-linking reactions (hardening) of the ink film are as follows:overprintable 20 °C 20 min 60 °C 5 min 120 °C 3 min stackable 20 °C 60 min 60 °C 20 min 120 °C 10 min final hardness 20 °C 5 days The times mentioned vary according to the substrate, the ink film thickness, the drying conditions and the selection of the auxiliaries used. Generally, an extended drying time is necessary when overprinting the ink. For multiple printing, please note that the film should not be completely cured before being overprinted.
If cured at a room temperature of 20 °C, the ink film has to be overprinted within 24 hours. Heat-activated intermediate curing is possible at 60 - 80 °C for 5 min.Printing parameters:
All types of commercially available fabrics and solvent-resistant stencils can be used. We re-commend a fabric between 48–70 and 68-64.
CONTACT US
Marabu printing inks are used all over the world - with 16 subsidiaries worldwide and distribution partners in more than 80 countries. Find your contact here.